Lead: 19,000 ppm · Cadmium: 200 ppm · Arsenic: not measured
19,000 ppm lead detected. While lead in fired ceramic glaze is generally tightly bound, at this concentration leaching into acidic foods (tomato, citrus, vinegar) becomes a realistic concern even in well-fired ware. FluoroSpec will confirm whether lead is surface-reactive. Also: 200 ppm cadmium present.
What XRF actually measures (and what it doesn't)
XRF detects elemental lead presence on the surface. It does not measure whether that lead migrates into food. Those are different questions. Lead bound in fired ceramic glaze is chemically locked in the vitreous matrix and, in independent leach testing on items up to ~3,000 ppm, showed no detectable migration. Lead in surface paint, decals, or worn glaze behaves very differently and is a meaningful exposure risk.
What this XRF reading actually means →
Test your own dishes with FluoroSpec →
Source data: independent consumer-safety researcher (factual data; verdict by EverythingLead)
Original source: https://tamararubin.com/2021/12/val-dol-sol-made-in-portugal-orange-glazed-ceramic-mug-19000-ppm-lead-please-do-not-use-ceramics-from-portugal-for-food-use-in-the-absence-of-independent-testing/
Test method: XRF (Niton XL 5 Plus, 1.5 sigma)
License: Factual XRF measurements are not copyrightable